r/Silvercasting • u/Fierro_nights • 5d ago
Casting thak test
Enable HLS to view with audio, or disable this notification
Testing casting thicker piece with same resin mix, royal blue and erilles
Used 3” flask filled just to cover print, bench rested 7 hrs while sleeping.
Burn out 100c 2hrs then 700c @ 1.5hr and 30m at 650.
10
Upvotes
1
u/Fierro_nights 5d ago
Also the prestige mixture used is 38/vanilla mix
1
u/Fierro_nights 5d ago
Also got a magnetic polisher doing some of the stuff Iv been casting recently just can’t get into spots reasonably the things pretty nice.
1
u/Fierro_nights 5d ago
So this dude is paying premium for a res thats not working out for the design well.
This is one of the deals and I know I’m doing it it would prolly be helpful if others did so as well. Log the res you use if using res, mixture and burn out schedule to help others.
Some res may need a dedicated flask and burn out vs a casting place doing other peoples shit all combined one dudes got wax and another one res and someone else a diff res etc. that’s bs. Fucking the whole damn tree up
1
u/Fierro_nights 5d ago
Wanted to update this thing, one of the things I’ve come across recently is where I mention the texture in the back of the hat. Some bits like that seems more of a bit of flux goes into the pour.
1
u/beepollenart 5d ago
Hotter for longer my burnout takes about 14 hours and it’s always clean. I use wax and polycast
1
u/undisclosed-identity 5d ago
This looks good! Admittedly, I don’t really understand some of the details. Since I don’t cast my own. I just design and print the x-wax and take it to the casting house.
What was the investment you used? I’ve heard that there are investments that work better for Bluecast and castable resins.