r/StainedGlass • • 2d ago

Help Me! Beginner help

Hi all!
These are my 3rd/4th solo pieces after doing a 6 week glass course (Aus based). Loving it so far!
I’m after some advice with solder as I’m getting mixed results. For context: both pieces are photographed before cleaning.
I’m struggling to get clean and shiny solder lines. Particularly on the geometric piece, the solder is super cloudy and dirty looking, whereas only some lines on the flower piece are shiny and clean. Even after giving them a good wash with dish soap and warm water, the lines on the geometric piece were still murky. I’m also finding that no matter how well I burnish the tape (and I’m not half-assing the process) the tape seems to lift when I solder.
What am I doing wrong?!

I’m using a Hakko T600FX soldering on 420° for main lines and 370° for edges, with Novacan liquid flux and unbranded copper tape (came as part of a kit from an art glass store).
Patterns from Lucent Glass

54 Upvotes

10 comments sorted by

6

u/Claycorp 2d ago

Lifting like this is normal and doesn't hurt anything. Getting more solder on at once and working the joint less will help with it. You can also push the foil back down with the iron when going over the joint.

The cloudy part is oxides floating on the surface of the solder and sticking. You need to clean your iron more often.

1

u/Miss_Pips 2d ago

Awesome, thank you for the advice!
Would you say I am soldering too hot or is that not a big factor in this issue?

2

u/Claycorp 2d ago

no. 410 ish is common. just make sure you are working fast enough.

3

u/Fun-Association340 2d ago

Im having the same issue, I have been having a look and i think my iron is contaminated. You can Apparently get a brass iron cleaner (looks like steel woolish) and a tip tinning powder. I use edco foil.

1

u/Miss_Pips 2d ago

Glad I’m not alone in this!
I have a brass wool iron cleaner but maybe I’m not using it often enough?

1

u/redthroway24 2d ago

I highly recommend flux gel. Stays in place longer. Are you planning to patina these pieces?

1

u/Miss_Pips 2d ago

I haven’t worked up the courage to use patina yet so I was just going to leave them silver for now!

3

u/Tetravex09 2d ago

Giving the pieces a good scrub with some baking soda helps get rid of extra flux and can really brighten the solder lines

2

u/indigo_mermaid 2d ago

I’ll also use a very fine steel wool to polish the solder before applying wax

1

u/ZookeepergameOne7168 2d ago

I just started myself, and just finished my second piece which I ran at 365° C and used gel flux. Before I completed my first two projects though, I was using liquid flux on junk pieces getting to know the process. I was also soldering at 420° C and the foil seams/edges were lifting up just like yours seem to be doing. I’m still a novice with this art, but what I think was happening is the temp of the solder was too hot and the adhesive backing of the foil was melting off the glass edge and lifting up. So that could be what was happening. Just my thought. Could be wrong. Have you tried soldering the main lines at a lower temp to see if it’s the temperature or the flux creating the problem?