r/Taxidermy • u/Repulsive-Basis9217 • 8m ago
Fur/Pelt Help Coyote hide tanning help!
Hey gang, i’m gonna tan a coyote fur for the first time (i’ve never tanned anything before). Been doin tons of research and i’ve decided to use some trubond chemicals to tan heard good things about trubond 1000b keeping hides really supple and soft. Few questions that I am unsure of
Salting before pickling even if my hide is frozen? - some seem to say that is it a key aspect of the process to reduce hair slippage and bacterial growth but others mentioned if you have your hide frozen there is no need to salt and you can just flesh it and go straight to the pickle? (I did buy lipa solve 55 so I could salt and then do a rehydration bath, im just unsure if this is necessary it would be 1/4lb salt:1 gallon water:1 oz lipa solve)
Deodorizer, do I need to add one to the pickle or is a simple degreaser bath okay? I got Lipa Solve 77 and plan to do a degreasing bath after the pickling and second fleshing and then i’ll throw it back into the pickle for a day after the degrease bath. Do I need deodorizer in the pickle as well? if so what brand do you recommend?
My plan so far is to:
- from freezer -> thaw
- 1st fleshing
- pickle 3 days? (3oz citric acid : 1lb salt : 1 gallon water) along with a bit of lipa solve 77 (1oz for 5 gal)
- second fleshing
- degreaser bath 3 hrs ( 1 gal water :0.5lb salt : 1oz lipa solve)
- quick warm water rinse
- pickle 1 more day
- neutralize bath (1/4lb salt:2oz baking soda:1gallon water)
- trubond 1000B brush on tan (working every 12hr till dry)
Any advice or recommendations are welcome! Thanks