Nice, did you polish the metal yourself? I wonder how well would such mirror surface stay shiny, given it's not touched.

3

u/Infrequentredditor6 Osmium Fanatic 3d ago

It was a coarsely ground wafer when I bought it. I used printer paper alone to sand it to a mirror finish, and I use Mother's Mag and Alum polish to keep it shiny. It fogs up with oxides over time, even in storage.

4

u/Ok-Literature-3997 Radiated 3d ago

That's very clever, good job. Very rare to see a mirror polished magnesium sample.

I've had worked with magnesium alloys some time ago and the only thing I remember is how awful those were to prepare for microscope work. Everything corroded them- the coolant, water, polishing compounds... Bonus points when you're polishing magthor and have to choose between lung cancer and wet, oxidized metallographic cross-sections.

I think I'm gonna go and polish my magnesium ingot now lol

3

u/Infrequentredditor6 Osmium Fanatic 3d ago edited 3d ago

That's actually pretty funny. You know what's even funnier?? Cold HF-nitric mixture will vigorously dissolve tungsten, but it will not dissolve magnesium, doesn't even appear to tarnish.

Yeah pretty much anything "wet" will react with it in some form or other. Someone on this subreddit said they clean magnesium with super dilute HCl. I tried it with this mirror because it makes for a very sensitive test—doesnt work. In fact there's still some slight remnants of corrosion from that even after polishing.

3

u/Ok-Literature-3997 Radiated 3d ago

But nitric alone would dissolve it, right? I think the lack of reaction is caused by very stable fluoride passivation.
I clean magnesium with very dilute vinegar and it works perfectly for unpolished pieces. No idea how would the mirror behave though, the vinegar acts rather quickly.

3

u/Infrequentredditor6 Osmium Fanatic 3d ago edited 3d ago

It's absolutely the fluoride passivating it, because nitric alone 100% will gobble it up.

I wouldn't trust even the slightest dip in pH to benefit that mirror. Even if it stays shiny the surface tarnishes. And plain water can make it go cloudy too. It's very sensitive, but the polish helps protect it from air for a while at least.