r/formlabs • u/blacklabel7 • 7d ago
Fuse+ Alternative cooling method?
I have a Formlabs Fuse+ SLS that I am running pretty hard. Build chamber is typically a 13-14 hour print and then a 7 hour cool down period.
I am well aware of all of the specs and recommendations that Formlabs provides about cooling times and post processing/quality concerns.
What i would like to do is run a build, pull the chamber out 15-30 minutes after it’s done, put it in a insulated environment or something to allow it to cool down and put my second chamber in right away to start the next build.. Has anyone done something like this? Wondering if a bench top programmable oven would work here or like a glass kiln or even some heavy duty specially insulated blankets..? Would be delighted to hear from others before I commit to any strategy.
Thanks
2
u/Joejack-951 7d ago
A PID controller and an oven big enough to fit the chamber ought to do it. Log the temperature data post-build from the Fuse then copy those settings using the controller. You might need to add a fan or two depending on how Formlabs does it.
2
u/Phoenixhawk101 3d ago
Yes,it is done. I know several companies that do this on the regular. On the right hand side door (where the air filters are) is a handle to manually open the door before the cool down trigger.
Then go find a local subway sandwiched shop that is cycling out their bread warmers (they have to do this every few years), their bread warmers are great because they get up around 120C and can store up to 4 build chambers (2 on the top shelf and 2 on the bottom).
1
u/Morin-3D 7d ago
You only need to cool to 100C before you can move the chamber to the sift, takes about an hour from the print ending afaik