r/metallurgy • • 5h ago

Brass

Post image
37 Upvotes

I see that we are sharing pictures of brasses, I have a huge collection of copper zinc aluminum shape memory brass pictures. This one is a single crystal of austenite, which transform into martensite upon cooling, what do you think?


r/metallurgy • • 1d ago

Warm Superconductor help needed to melt silicon and zinc with a third element in the middle.

0 Upvotes

r/metallurgy • • 1d ago

I need help making a warm superconductor that requires very specific melting temperatures for elements like zinc and silicon with a third element in the middle.

0 Upvotes

r/metallurgy • • 1d ago

DIY metallographic microscope using 3D glasses and a traditional stereo microscope

7 Upvotes

It’s a bit makeshift, but it works.

In the previous photo I used a different microscope


r/metallurgy • • 1d ago

METALURGIA

Post image
1 Upvotes

r/metallurgy • • 2d ago

My metallographic microscope dates back to 1952; it’s a biological model, but you can attach additional components for phase contrast or fluorescence...

Post image
10 Upvotes

r/metallurgy • • 2d ago

Ideas for at home metallography preparation?

6 Upvotes

Solved, thank you!

Hey folks! I’m loving all the microstructures I’ve been seeing lately and wanted to join in!

When I take pictures of the structure after an etch, the pictures are ruined by these micro scratches that come from lower grits on my belt sander.

What kind of polishing set ups do you guys have?

I have a belt sander that goes up to 400 grit sand paper followed by a buffing wheel with varying fineness buffing compounds.

I’ve seen a lot of metallography polishing kits online with rotating sanding disc as opposed to a belt sander (Kalamazoo 2x48in) like I have. This grinder only has one speed option which works best for hogging metal off for cleaning up and flattening ingots.

Thanks!

Edit: I saw those kits online that cost about $3k that I’d like to avoid spending if possible


r/metallurgy • • 2d ago

brass + vinegar + hydrogen peroxide + ferrous sulfate....

Thumbnail
gallery
14 Upvotes

r/metallurgy • • 2d ago

brass, brightfield and darkfield + polarization

Thumbnail
gallery
8 Upvotes

I’ll try changing the etchant.


r/metallurgy • • 2d ago

Ich bin auf einen interessanten Anwendungsfall aus der industriellen Instandhaltung gestoßen.

Post image
0 Upvotes

r/metallurgy • • 2d ago

No tithe needed

Thumbnail
reddit.com
0 Upvotes

r/metallurgy • • 2d ago Bravo

Hopping onto the brass metallography trend here are some micrographs I took on annealed cartridge brass

Thumbnail
gallery
212 Upvotes

Started with a half hard brass rod that I recrystallized to try and maximize grain growth. Etched with a HCl and ferric chloride solution . First and third images are with polarized light and second is bright field.


r/metallurgy • • 3d ago

Can a metallurgist tell me how to find the right metal to manufacture the right kind of hand tool ? And how to test these tools

0 Upvotes

I am a trader of hand tools, after I die, I want to leave humanity with a brand of tools that is genuinely value for money, but I realized I don’t know jackshit about metals, all the pliers look the same, so does all the bits .. you never know which are good quality. So I think only and metal engineer can give me some insight.


r/metallurgy • • 3d ago

Polished brass + Klemm’s reagent

14 Upvotes

r/metallurgy • • 3d ago

Brass

14 Upvotes

r/metallurgy • • 3d ago

Experimenting with plating

Thumbnail gallery
7 Upvotes

r/metallurgy • • 3d ago

What kind of surface treatment is this?

Post image
2 Upvotes

What kind of surface treatment/ coating is in this grey band area. This surface is used as a counter face for oil seal lip.

Can you also suggest any alternative to this?


r/metallurgy • • 4d ago

The Metallurgy of HAFNUM

Thumbnail gallery
74 Upvotes

Complete with spelling mistake, big thumbs little phone


r/metallurgy • • 4d ago

Can I work in metallugy even if I'm disabled?

9 Upvotes

I have scoliosis which makes standing for hours on end somewhat difficult. I'm also a 5'3 woman who struggles to life heavy weights. In addition to all of that, I'm on mental health medication that makes me somewhat heat intolerant. I'm currently pursuing a degree in metallugical engineering, I'm a junior now and I thought that these things would be fine since engineering tends to be somewhat disability friendly, however I'm trying to pursue an R&D internship for the summer. This internship requires a physical and I'm unsure if I'll pass it due to my heat intolerance and carrying 50 pounds for 10 minutes. This has totally made me rethink everything, should I continue trying to get this degree, or do I need to pivot to some other type of engineering or other job entirely.


r/metallurgy • • 5d ago

Shaft fractured analys - what do you think caused this failure?

Thumbnail
gallery
27 Upvotes

This shaft failed right through the keyway, and I'm trying to figure out the root cause. Looking at the fracture surfaces, it seems fairly abrupt without obvious fatigue beach marks, though there is a key/keyway feature near the edge. What do you think caused this break (overload/shock, torsion/shear, stress concentration at the keyway, or fit/play issues)? I’d really appreciate it if you could point out what specific features you see on the fracture surface so I can learn how to read these better in the future.


r/metallurgy • • 5d ago

Advice to save important rings

Thumbnail
gallery
5 Upvotes

I'm looking for some experts to guide me to help take the best care of very important rings I have.

The story behind the rings is that they were brought by my boyfriend as a birthday gift last year. We were so in love and planning to get married and start our family soon but unfortunately he died in an accident a few months ago and these rings are one of the few things I have from since his family refused to acknowledge our relationship and took away everything that belonged to him. These are 100% zinc rings from H&M he bought cause we were broke back then lol but we were planning the wedding together so now these are the only engagement rings I'll have so can someone please help me know how to take care of these rings they are already tarnished and Google didn't help now I'm fearing I'll loose them too. Thank you in advance to any kind person who can guide me 💜💜🌻🌻

Link to the similar rings: https://www2.hm.com/en_in/productpage.1352041001.html


r/metallurgy • • 6d ago

aluminum alloy (silumin)

39 Upvotes

r/metallurgy • • 7d ago

Recommendations for a failure analysis outfit

9 Upvotes

Good afternoon. I was wondering if anyone here could recommend an outfit (business/lab/etc) that I could sent a sample of a failed shaft to for a detailed failure analysis.

*Backstory* - We have an OEM supplier that has a corner on the market for a specific industrial machine. The business I work for has many of these machines and over the last year we have had three high profile shaft failures (quite uncommon normally). The OEM does not seem interested in helping to identify the cause of the failures or assist in any changes that might mitigate further issues. So we looking to get some outside *expert* help to hold them accountable if there is some kind of defect or substandard supply.

These shafts are large 10 inch or so in diameter and 15 ft or so ft long. I am sure we would be willing to have a section with the failure points cut down to be sent out for testing.

Any recommendations? We are in Texas if that helps.


r/metallurgy • • 10d ago

Failure Analysis Questions

Thumbnail
gallery
112 Upvotes

I am currently working on doing failure analysis for a crankshaft made of forged and surface hardened 4140 steel. The crankshaft delivers power to a die which is used to cut metal tubes. I have attached photos of both sides of the fracture surface, and my own annotations.

My current thought is that this is a rotary bending fatigue case, where the sudden reduction in diameter between the two parts of the crankshaft created a stress concentration at the keyway. Is my analysis any good?