r/InjectionMolding • • 4d ago

Troubleshooting Help Help. Core support mid injection.

Having a proplem with a mold that has loong slider that bends due to injection pressure. Many thing have been tried to balance the flow and change the placement of the injection but with not big improvement. I have suggested if the core would be supported with a slider thats hydraulic. The slider would support the other slider for 80-90%(or whatever is the best ammount) of the injection cycle and then stop supporting and slide to be part of the mold surface. They said the machine cant do that kind of function mid injection, it could but they have not paid for that kind of function. So im asking if anyone has experience how this could be still done.

Im confident that its the right way to surpass this problem because another company uses it in a really similar part.

Edit: changed the core word for slider.

5 Upvotes

31 comments sorted by

1

u/Galleom64 4d ago

What material? What temps? What speed?

And what do you mean bends?

1

u/mizyks 4d ago edited 4d ago

Its a pipe mold. The wall thickness changes due to long slider that has no support its close to a meter and 28mm diametre. Materials that have been tried are pp and abs. I cannot give the temps and speed because they have been changed so many times, and im no molder, i'm a toolmaker. But slower speed= is better but it cannot be injected slower.

2

u/fosterdad2017 4d ago

Hahaha... thats fucked, good luck.

I've done this a few times. If the mold cannot be any stronger and better supported, you'll need more plastic wall thickness.

Even perfect fill balance will push everything out of alignment at the last bit of pack. If you can get to 98% filled parts with no imbalance in flow front or wall thickness, you have proof the mold is not strong enough.

Support the cores for a length 1.5 to 3x the diameter on a 5-10 degree taper or else the tool design is deficient.

1

u/mizyks 4d ago

I know haha. The wall thickness should be around 2mm cannot be changed and tbh the minium wall thickness has been at1.3mm and 1.4mm. Thats already suprising.

3

u/fosterdad2017 4d ago

Just because the customer wants it, doesn't make physics allow it.

Check your L/T ratio. If 800mm and 1.3mm thats 615:1 flow length and perfectly 100% impossible. Reduce below about 300:1 by increasing plastic thickness or making the part shorter.

1

u/mizyks 4d ago edited 4d ago

But we have already made parts that had minium 1.3mm wall thickness. Customer just does not like it because it bends after cooling due to different wall thickness. But another material than pp could help with that. And for the flow balance haha. I made banana/cashew gates on top of the pipe in the injection side and also on the ejection side. Looked pretty wild

1

u/mizyks 4d ago edited 4d ago

And yes its 2 cavity mold😂

1

u/fosterdad2017 4d ago

Doesn't work. Make the core rigid, align the mold halves with mega strong interlocking, telescope the core if possible.

1

u/mizyks 4d ago

Maybe core is wrong word. Its a slider. 800mm long and 28mm diametre. Also there is another slider 300mm long they form an L shape.

1

u/rustyxj 4d ago

Does one slide shut off onto the other slide?

Easy fix for that is to make them interlock, grind a bullet on the tip of the core that extends, and put a tapered hole for it to mate to on the other end.

1

u/mizyks 4d ago

Yes. Well they have "interlock" but its still not supported in other directions.

1

u/mizyks 4d ago edited 4d ago

The L curve is rigid. But it still has two directions of non supported movement.

1

u/mizyks 4d ago

What do you mean it would not work? Not working without the chance to operate hydraulics mid injection or just in general? And why?

1

u/fosterdad2017 4d ago

I've built this idea. The imbalance force is extreme. Locked up the tool, hobbed the supporting cores into the main core steel. You cant solve the problem this way.

1

u/mizyks 4d ago

But if it would be supported mid injection the solified plastic would help support it at the end of the injection cycle, It could leave leave a mark because the plastic would need to fill the void that the support creates but i see no problem on the part. i have one part that have analysed that im sure uses this kind of way and the mark is really small.

1

u/mizyks 3d ago

But since you have build this idea, would you mind giving me a dm? Would wanna know more about it. Not sure we are trying to do it that way, but still want to learn if there is a possibility to do it in some future parts. We a have another idea that has shown some results but needs further testing and is unrealiablea in it's current state

1

u/flambeaway 1d ago

Could try Kentucky windage? Make a bent core that will deflect to into the shape you want, lol.

1

u/mizyks 1d ago edited 1d ago

Haha you known what we tried it sorta. There is a 14mm cooling hole inside the slider. We bended 13.9mm rods and then hardened them and shoved them in. The result was small/unnoticable,which was kinda expected. when you are trying to stiff the slider by 100% with a 14mm axel goes without saying its not gonna work. But i think some people were hoping for a miracle. There is one thing we are tryong next but its again pretty wild. The support mid injection is in my mind the way to go, since there is similar product on market and it has been done that way imo. But i have no experince on this kind of system and would like to know if there is something that would be good to know before manufacturing it.

1

u/moldingHELP 4d ago

Your idea of having a moving core at the end to support the long core is absolutely doable and has been done for decades very successfully. External control of this is very simple as well.

Feel free to contact me if you would like to discuss this further. External control of this is very simple as well. My name is Kip Doyle and my company is moldingHELP. (Google me for contact information.)

1

u/rustyxj 4d ago

Yeah, you've got a core that's like an inch thick and 31.5" long, whoever designed this is an idiot.

1

u/mizyks 4d ago

Well its a pipe mold, you cant really do it otherway. The sliders also have zero draft. But atleast there is compressed air coming on the tip of the slider so that helps.

2

u/rustyxj 4d ago

Well its a pipe mold, you cant really do it otherway.

I'd extrude it like the rest of the world does.

3

u/mizyks 4d ago

Extrude and bend. That what i said after i heard about the project. Too expensive and labor intense. Better to have mold that does not work

1

u/rustyxj 4d ago

Oh shit, I didn't see the part where you said there is a bend in it.

I feel like it would have saved them a shit ton of money if they would have extruded then bent it.

1

u/mizyks 4d ago

Well yes. But when you are injection mold company. Everything needs to be done that way.... But im sure it could work. The wall thicknees should be 2mm. Now we have been at 1.3mm minium but the plastic bends when it cools so its a nono. Maybe material change could help with that.

But we are still at the point that anything over 25% difference is un acceptable.

1

u/rustyxj 4d ago

Well yes. But when you are injection mold company. Everything needs to be done that way....

Gotta diversify, not everything needs to be molded,

3

u/mizyks 4d ago

Ooh and yes, there is extrusion already. The bending was a nono, because no machine🫣 but also im not here to talk how fucked up this is. Just trying to make it work haha

2

u/rustyxj 4d ago

Good luck, from one toolmaker to another, I know how bad engineering can be sometimes.

2

u/mizyks 4d ago edited 4d ago

Thanks.. it's just too ambious part. Actually just shortening the part may be the right way to go, not that hard to modify. But then its not the longest part on known market that has been made this way. Certainly it would be easiest way😅 shortening unsupported part by 100mm would already make a big difference. All the things that has been modified would also make bigger difference. But then again, i'm curiois about the way the sliders could be supported mid injection and how the end result would be, seems possible but not much info found. Only some patents on golfball injection molding that uses that kind of way to overmould entire balls. + Some written solutions and analysis. But i have a similar part that has hints of similar production method.

1

u/mizyks 4d ago

I know. There were words like that said.

2

u/Piffigan 4d ago

I don't know a lot about the technical side as I'm a toolroom apprentice but at our place we had a similar job, a bent pipe and we ran it on gas almost like blow moulding and machines off the ends but obviously the tool was designed for that in the first place